Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 8.40 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 1000 °C
4.67 µin/in-°F

@Temperature 68.0 - 1830 °F
60° to c-axis
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
CTE, linear 8.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.67 µin/in-°F

@Temperature -22.0 - 158 °F
Schott K7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.67 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BAF51 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.67 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-BALF5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.67 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LASF9 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.67 µin/in-°F

@Temperature 68.0 - 572 °F
Schott SF10 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.67 µin/in-°F

@Temperature -22.0 - 158 °F
Schott SF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 300 °C
4.67 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAF7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.40 µm/m-°C

@Temperature 25.0 - 1000 °C
4.67 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
CTE, linear 8.40 µm/m-°C

@Temperature 30.0 - 800 °C
4.67 µin/in-°F

@Temperature 86.0 - 1470 °F
Ametek Molybdenum-Copper Composite AMC 7525
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
Copyright © lookpolymers.com All Rights Reserved