Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.80 µm/m-°C @Temperature 25.0 - 100 °C |
4.33 µin/in-°F @Temperature 77.0 - 212 °F |
|
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 900 °C |
4.33 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton EXP 36 Cordierite Mullite REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.33 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAF52 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.33 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott UG11 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KZFS8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 20.0 - 600 °C |
4.33 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 20.0 - 1000 °C |
4.33 µin/in-°F @Temperature 68.0 - 1830 °F |
ASTM-C372 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
CTE, linear | 7.80 µm/m-°C @Temperature 30.0 - 150 °C |
4.33 µin/in-°F @Temperature 86.0 - 302 °F |
|
Ametek Molybdenum-Copper Composite AMC 7525 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |