Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.3 µm/m-°C @Temperature <=871 °C |
11.3 µin/in-°F @Temperature <=1600 °F |
|
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature <=871 °C |
11.3 µin/in-°F @Temperature <=1600 °F |
|
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 50% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 20.3 µm/m-°C @Temperature 20.0 - 871 °C |
11.3 µin/in-°F @Temperature 68.0 - 1600 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |