Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.0 µm/m-°C @Temperature 1000 °C |
11.1 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 1000 °C |
11.1 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 1000 °C |
11.1 µin/in-°F @Temperature 1830 °F |
|
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 250 °C |
11.1 µin/in-°F @Temperature 482 °F |
|
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature >=143 °C |
11.1 µin/in-°F @Temperature >=289 °F |
ISO 11359 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature <=143 °C |
11.1 µin/in-°F @Temperature <=289 °F |
ISO 11359 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 |
Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy Xtel® XE4050BL is a glass fiber and mineral filled PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevron Phillips.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 21.0 - 871 °C |
11.1 µin/in-°F @Temperature 69.8 - 1600 °F |
|
Crucible Steel XM-19 Stainless Steel Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 100A Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature -14.0 - 38.0 °C |
11.1 µin/in-°F @Temperature 6.80 - 100 °F |
ASTM D696-91 |
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 100VN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 100ZT Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 200A Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ar.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 200EN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications requ.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 200FPC Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thickn.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature -14.0 - 38.0 °C |
11.1 µin/in-°F @Temperature 6.80 - 100 °F |
25 µm film; ASTM D696-91 |
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an .. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 500VN Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available .. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available .. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 50VN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 100FPC Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 25.6 - 871 °C |
11.1 µin/in-°F @Temperature 78.0 - 1600 °F |
|
Carlson Nitronic® 50® Austenitic Stainless Steel General DescriptionNitronic 50 is a nitrogen-strengthened austenitic stainless steel that possesses corrosion resistance superior to 316, 316L, 317 and 317L plus approximately twice the yield streng.. |
|||
CTE, linear | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
Value for Kapton® HN |
DuPont™ Kapton® 200VN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available in.. |