Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 144 µm/m-°C @Temperature 200 - 300 °C |
80.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
CTE, linear | 144 µm/m-°C @Temperature <=100 °C |
80.0 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
CTE, linear | 144 µm/m-°C @Temperature 150 - 200 °C |
80.0 µin/in-°F @Temperature 302 - 392 °F |
Alpha 2 |
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc. |
|||
CTE, linear | 144 µm/m-°C @Temperature 100 - 150 °C |
80.0 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-00 |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |