Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.2 µm/m-°C @Temperature 204 °C |
6.80 µin/in-°F @Temperature 400 °F |
x-ply; 8HS form; ASTM D696 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 0.000 - 300 °C |
6.78 µin/in-°F @Temperature 32.0 - 572 °F |
|
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 500 °C |
6.78 µin/in-°F @Temperature 68.0 - 932 °F |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 300 °C |
6.78 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 500 °C |
6.78 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 500 °C |
6.78 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 500 °C |
6.78 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 500 °C |
6.78 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 700 °C |
6.78 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 300 °C |
6.78 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 538 °C |
6.78 µin/in-°F @Temperature 1000 °F |
|
Special Metals INCOLOY® alloy 908 INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.80 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 21.1 - 427 °C |
6.80 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel 161 Tool Steel, High Carbon H13 Crucible 161 is a high carbon modification of H13, intended for applications requiring higher hardness, compressive strength, wear resistance, or tempering resistance (hot hardness), at slightly low.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 21.0 - 300 °C |
6.78 µin/in-°F @Temperature 69.8 - 572 °F |
Mean |
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 300 °C |
6.78 µin/in-°F @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology... |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 300 °C |
6.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 600.0 °C |
6.80 µin/in-°F @Temperature 1112 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 21.0 - 316 °C |
6.78 µin/in-°F @Temperature 69.8 - 601 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 500 °C |
6.78 µin/in-°F @Temperature 68.0 - 932 °F |
|
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2) Speed Star high speed steel in a fine-grained "Moly"-Tungsten high-speed steel manufactured under close control. It has certain advantages over 18-4-1 high speed steels, some of which are lower cost.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 300 °C |
6.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 25.0 - 700 °C |
6.78 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 204 °C |
6.78 µin/in-°F @Temperature 68.0 - 399 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 21.1 - 399 °C |
6.80 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |