Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 71.0 - 88.0 µm/m-°C @Temperature 55.0 - 320 °C |
39.4 - 48.9 µin/in-°F @Temperature 131 - 608 °F |
Average value: 84.1 µm/m-°C Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
CTE, linear, Transverse to Flow | 72.0 - 88.0 µm/m-°C | 40.0 - 48.9 µin/in-°F | Average value: 80.0 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear, Transverse to Flow | 88.0 - 88.0 µm/m-°C @Temperature 60.0 - 138 °C |
48.9 - 48.9 µin/in-°F @Temperature 140 - 280 °F |
Average value: 88.0 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |