Polymer Property : CTE, linear, Transverse to Flow = 74.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 134 µm/m-°C

@Temperature 20.0 °C
74.4 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 383A-08 Cellulose Acetate Propionate  (discontinued **)
8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Transverse to Flow 134 µm/m-°C

@Temperature 23.0 - 60.0 °C
74.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East)
LNP* Lubricomp* ML003 is a compound based on Polypropylene resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 134 µm/m-°C

@Temperature -30.0 - 30.0 °C
74.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.
CTE, linear, Transverse to Flow 134 µm/m-°C

@Temperature 20.0 °C
74.4 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.