CTE, linear, Transverse to Flow 30.0 - 96.0 µm/m-°C
16.7 - 53.3 µin/in-°F
Average value: 70.1 µm/m-°C Grade Count:11
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
CTE, linear, Transverse to Flow 80.0 - 96.0 µm/m-°C
44.4 - 53.3 µin/in-°F
Average value: 86.1 µm/m-°C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
CTE, linear, Transverse to Flow 83.0 - 96.0 µm/m-°C
46.1 - 53.3 µin/in-°F
Average value: 90.7 µm/m-°C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
CTE, linear, Transverse to Flow 96.0 - 96.0 µm/m-°C

@Temperature 55.0 - 160 °C
53.3 - 53.3 µin/in-°F

@Temperature 131 - 320 °F
Average value: 96.0 µm/m-°C Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..