Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 32.0 - 90.0 µm/m-°C | 17.8 - 50.0 µin/in-°F | Average value: 58.3 µm/m-°C Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear, Transverse to Flow | 69.0 - 90.0 µm/m-°C | 38.3 - 50.0 µin/in-°F | Average value: 75.1 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 90.0 - 90.0 µm/m-°C @Temperature 100 - 200 °C |
50.0 - 50.0 µin/in-°F @Temperature 212 - 392 °F |
Average value: 90.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
CTE, linear, Transverse to Flow | 6.30 - 90.0 µm/m-°C | 3.50 - 50.0 µin/in-°F | Average value: 61.0 µm/m-°C Grade Count:16 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
CTE, linear, Transverse to Flow | 30.0 - 90.0 µm/m-°C | 16.7 - 50.0 µin/in-°F | Average value: 75.0 µm/m-°C Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 90.0 µm/m-°C | 22.2 - 50.0 µin/in-°F | Average value: 73.6 µm/m-°C Grade Count:39 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear, Transverse to Flow | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Average value: 80.0 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |