Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 36.0 - 60.0 µm/m-°C | 20.0 - 33.3 µin/in-°F | Average value: 50.3 µm/m-°C Grade Count:14 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |