Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 81.2 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |