Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 34.0 - 62.0 µm/m-°C @Temperature 55.0 - 260 °C |
18.9 - 34.4 µin/in-°F @Temperature 131 - 500 °F |
Average value: 47.7 µm/m-°C Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 62.0 µm/m-°C @Thickness 2.00 - 4.00 mm |
18.9 - 34.4 µin/in-°F @Thickness 0.0787 - 0.157 in |
Average value: 47.7 µm/m-°C Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 2980 µm/m-°C | 18.9 - 1660 µin/in-°F | Average value: 473 µm/m-°C Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 100 µm/m-°C | 18.9 - 55.6 µin/in-°F | Average value: 66.3 µm/m-°C Grade Count:24 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature 20.0 °C |
18.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baygal® 90 IK 20 Polyurethane Uses: Suitable for the production of parts: for example: insulators, bushing insulators, components of switchgear cabinets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C | 18.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature 23.0 - 150 °C |
18.9 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8541 Polyimide Thermoplastic parts from filled PI (polyimide) for high mechanical properties and impact performance in high temperature environmentsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature 50.0 - 150 °C |
18.9 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 38.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
18.9 - 21.1 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 110 µm/m-°C | 18.9 - 61.1 µin/in-°F | Average value: 62.4 µm/m-°C Grade Count:3 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 34.0 - 76.0 µm/m-°C | 18.9 - 42.2 µin/in-°F | Average value: 51.7 µm/m-°C Grade Count:3 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature 20.0 °C |
18.9 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Thickness 1.60 mm |
18.9 µin/in-°F @Thickness 0.0630 in |
ASTM D696 |
E-Polymers SEPAZ® K130HF 30% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 42.0 µm/m-°C | 18.9 - 23.3 µin/in-°F | Average value: 38.7 µm/m-°C Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and ma.. |