Polymer Property : CTE, linear, Transverse to Flow = 156 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature -40.0 - 40.0 °C
86.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX MS002 PP
LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature -40.0 - 40.0 °C
86.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature -40.0 - 40.0 °C
86.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature 23.0 - 60.0 °C
86.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.