Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 134 µm/m-°C @Temperature 20.0 °C |
74.4 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 383A-08 Cellulose Acetate Propionate
(discontinued **) 8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 134 µm/m-°C @Temperature 23.0 - 60.0 °C |
74.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East) LNP* Lubricomp* ML003 is a compound based on Polypropylene resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 134 µm/m-°C @Temperature -30.0 - 30.0 °C |
74.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 134 µm/m-°C @Temperature 20.0 °C |
74.4 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |