Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 121SRM PC (Asia Pacific) Easy flow, impact modified, super release grade polycarbonate. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 123HSR PC (Asia Pacific) Easy flow, UV stabilised, super release grade polycarbonate. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 123SRM PC (Asia Pacific) Easy flow, uv stabilised, impact modified, super release grade polycarbonate. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 133 °C @Thickness 4.00 mm |
271 °F @Thickness 0.157 in |
Unannealed; ASTM D648 |
LG Chemical Lupoy 1320C-07 Polycarbonate Resin Description: LUPOY PC 1320C-07 resin provides stability against ultraviolet radiations to solid or multi-wall sheets via the coextrusion of a 50 ? thick layerMain Characteristics: Proprietary formul.. |