Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 6.40 mm |
491 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin Extem XH2315 Resin |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 6.40 mm |
491 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific) Extem XH2315 Resin |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 6.40 mm |
491 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East) Extem XH2315 Resin |