Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 150 - 343 °C | 302 - 649 °F | Average value: 171 °C Grade Count:11 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |