Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 216 °C | 420 °F | ASTM D3418 |
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet) |
|||
Glass Transition Temp, Tg | 216 °C | 420 °F | Wet |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |