Thermal Properties Metric English Comments
Glass Transition Temp, Tg 201 °C
394 °F
Onset
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS
Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel
Glass Transition Temp, Tg 201 °C
394 °F
Onset
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/IM7 GS
Fiber: IM7 GS, UD, 150 g/m2Information provided by HexCel
Glass Transition Temp, Tg 201 °C
394 °F
Onset
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/48370/1000
Fiber: HR 12K, 2x2 Twill, 370 g/m2Information provided by HexCel
Glass Transition Temp, Tg 201 °C
394 °F
Onset
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000
Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel