Thermal Properties Metric English Comments
Glass Transition Temp, Tg -16.0 °C
3.20 °F
Mallard Creek Polymers ROVENE® 4402 SBR Latex
ROVENE® 4402 is a carboxylated styrene-butadiene emulsion which does not contain nor evolve formaldehyde during cure. ROVENE® 4402 has a medium soft hand with outstanding strength properties. ..
Glass Transition Temp, Tg -16.0 °C
3.20 °F
Mallard Creek Polymers Rovene® 5051 Styrene-Butadiene Emulsion
ROVENE® 5051 is a medium-firm, self cross-linking, carboxylated styrene-butadiene latex emulsion. Its styrene content permits the use in formulating carpet and flooring mastics. This versatile po..
Glass Transition Temp, Tg -16.0 °C
3.20 °F
Mallard Creek Polymers Rovene® 6103 Resin Supported Emulsion
Rovene® 6103 is a soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6103 can be used as the film forming..
Glass Transition Temp, Tg -16.0 °C
3.20 °F
Inflection
Dow Advanta® 3302 Specialty Elastomer  (discontinued **)
Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000..