Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -5.00 - 155 °C
23.0 - 311 °F
Average value: 74.0 °C Grade Count:80
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
Mallard Creek Polymers ROVENE® 4100 SBR Latex
ROVENE® 4100 is a carboxylated styrene-butadiene emulsion designed to give excellent performance properties in air knife and blade coating formulations. ROVENE® 4100 exhibits the following per..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
ASTM E1356
SK Chemicals SKYTHANE® US130J Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
Styron XZ 92024.00 Cross-Linking SB
Performance Features: Excellent alkali resistance, low blockingApplications: Fiber Binding, Glass Fiber Binding and Performance CoatingsEuropeInformation provided by Styron
Glass Transition Temp, Tg -5.00 °C
23.0 °F
Unitika elitel UE3800 Polyester, Pellet
Hot melt adhesives, Adhesives for polyvinylchlorideUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesiv..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
Loctite® 3882 Flexible Isotropic Epoxy Adhesive
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
Loctite® Durabond® E-90FL Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Glass Transition Temp, Tg -5.00 °C
23.0 °F
MDSC, postcured
DuPont Performance Polymers VTR 8605 (GF-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **
FormulationVTR 8605