Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 98.0 °C | 208 °F | TM R050-25 |
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | |
Lucite International Elvacite ® 2010 Acrylic Resin Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides.. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | Ultimate Tg |
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se.. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | Ultimate Tg |
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se.. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | |
Armstrong C-7/H20 Epoxy Adhesive A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Glass Transition Temp, Tg | 98.0 °C | 208 °F | |
Armstrong A-3/E Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |
|||
Glass Transition Temp, Tg | 98.0 - 107 °C | 208 - 225 °F | Average value: 102 °C Grade Count:3 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |