Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS455-203 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | DSC |
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, .. |
|||
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | DSC |
Lubrizol Estane® 5712 Thermoplastic Polyurethane Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl.. |
|||
Glass Transition Temp, Tg | -39.0 °C | -38.2 °F | |
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod.. |