Thermal Properties Metric English Comments
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® PS 455-204 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
HR 10 K/min, half height
Styron Sprintan® SLR 6430 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-6430 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. In relation to solid rubber the grade is extended with 37.5 p..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
ASTM D3418
DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
Zeon Chemicals Hydrin® T3100 Polyepichlorohydrin Elastomer
Hydrin T3100 is an epichlorohydrin/ethylene oxide/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3100 typically exhibit good heat resistance, exc..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
DSC
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
DSC
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
DSC
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
10°C/min
Covestro Texin® 390 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
10°C/min
Arkema Group Kynar® FLEX 2800 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
10°C/min
Arkema Group Kynar® FLEX 2801 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
10°C/min
Arkema Group Kynar® FLEX 2821 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn..
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
10°C/min
Arkema Group Kynar® FLEX 2822 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness ..