Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -80.0 °C | -112 °F | |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Glass Transition Temp, Tg | -80.0 °C | -112 °F | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Glass Transition Temp, Tg | -80.0 °C | -112 °F | |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Glass Transition Temp, Tg | -80.0 °C | -112 °F | |
3M Scotchcast™ 2130 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it.. |
|||
Glass Transition Temp, Tg | -80.0 °C | -112 °F | |
3M Scotchcast™ 2136 Potting Kit The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat.. |