Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5621Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5640Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5641Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2179 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2145 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | ASTM D4065 |
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | ASTM D3418 |
Lubrizol Estane® UB400 Thermoplastic Polyurethane Type: Estane® UB400 is a Shore 78A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in AsiaI.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | |
Trelleborg Emerson & Cuming Stycast® E-1000 One-Component Epoxy Low Stress Encapsulant Emerson & Cuming E-1000 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | DSC |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | |
Zeon Chemicals Nipol® 1401LG Nitrile Powder and Crumb Elastomer Nipol 1401LG is a copolymer of butadiene and acrylonitrile of excellent oil resistance. This material is ground and dusted with approximately 2.0% mineral anticake which allows direct addition to mi.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | dynamic; DIN 53 736 |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |