Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 75.0 - 275 °C | 167 - 527 °F | Average value: 178 °C Grade Count:63 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |