Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 87.0 °C | 189 °F | ASTM D1525 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | ASTM D1525 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | DSC |
Kolon NOPLA® KE131 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | |
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea Description: Specialty monomer for Wet Adhesion PromotionIdentification: COMPOSITION BASED ON METHACRYLAMIDOETHYL ETHYLENE UREACAS: 3089 – 19 – 8Solubility: Total in water Polymer Test (10.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | Ultimate Tg |
Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for .. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | Onset, Cure Temperature: 140°C, Cure Time: 10 min |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy HexPly® M52 is a modified epoxy matrix with good mechanical and temperature performance, specifically designed for rapid press curing. HexPly® M52 is ideal for small to high volume industrial appl.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | |
Loctite® Durabond® E-20NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Glass Transition Temp, Tg | 87.0 °C | 189 °F | |
Armstrong A-3/A Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |