Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 17.0 °C | 62.6 °F | |
Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion BARRIER PRO® 4545 is an anionic carboxylated styrene-butadiene copolymer latex. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and pliable, cur.. |
|||
Glass Transition Temp, Tg | 17.0 °C | 62.6 °F | |
Mallard Creek Polymers ROVENE® 4041 SBR Latex ROVENE® 4041 is a freeze-thaw stable carboxylated styrene-butadiene emulsion that can be used as a modifier for concrete applications. Concrete modified with ROVENE® 4041 is much tougher, more.. |
|||
Glass Transition Temp, Tg | 17.0 °C | 62.6 °F | |
Mallard Creek Polymers TYKOTE® 1004 SBR Emulsion TYKOTE® 1004 is an anionic carboxylated styrene-butadiene copolymer latex. Features: exceptional water resistance, exceptional grease resistance, pigment compatible, very high tensile strength, .. |