Thermal Properties Metric English Comments
Glass Transition Temp, Tg 161 °C
322 °F
DMA (SYSS)
RedEye On Demand PC-ISO for Parts that can be Sterilized
Polycarbonate-ISO (PC-ISO) is a durable high-performance plastic that meets both ISO 10993-1 and USP Class VI standards in its raw state. PC-ISO can be sterilized using either the gamma radiation or..
Glass Transition Temp, Tg 161 °C
322 °F
DMA (SYSS)
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping
Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo..
Glass Transition Temp, Tg 161 °C
322 °F
DSC (SSYS)
Stratasys® Polycarbonate
A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts ..
Glass Transition Temp, Tg 161 °C
322 °F
DMA (SSYS)
Stratasys® Polycarbonate-ISO
PC-ISO (polycarbonate-ISO), an industrial thermoplastic, in its raw state meets the ISO 10993-1 and USP Class VI classification1 and comes in a variety of colors. Because of their strength and medic..
Glass Transition Temp, Tg 161 °C
322 °F
DAM (SSYS)
Proto3000 PC Fused Deposition Modeling Polymer
Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating ..
Glass Transition Temp, Tg 161 °C
322 °F
DAM (SSYS)
Proto3000 PC ISO Fused Deposition Modeling Polymer
Description: PC-ISO (polycarbonate-ISO), an industrial thermoplastic, which in its raw state, meets the ISO 10993-1 and USP Class VI classi?cation 1. PC-ISO blends are commonly used in food and drug..