Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -42.0 - -39.0 °C | -43.6 - -38.2 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -42.0 - -39.0 °C | -43.6 - -38.2 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | |
Mallard Creek Polymers ROVENE® 4813 SBR Emulsion ROVENE® 4813 is a high gel content hot polymerized SBR latex with 30% bound styrene content. It has excellent shear stability and high tolerance for fillers and pH shock. It is easily tackified a.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | |
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | |
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | DSC |
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | 10°C/min |
Covestro Texin® 285 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Glass Transition Temp, Tg | -42.0 - -40.0 °C @Frequency 1.00 Hz |
-43.6 - -40.0 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | 10°C/min |
Arkema Group Kynar® 9000 HDC N 123 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | DSC |
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer Product Description: Exxelor VA 1801 polymer resin is a medium viscosity, semi-crystalline ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone.. |
|||
Glass Transition Temp, Tg | -42.0 °C | -43.6 °F | |
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l.. |
|||
Glass Transition Temp, Tg | -42.0 - -40.0 °C @Frequency 1.00 Hz |
-43.6 - -40.0 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |