Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -10.0 °C | 14.0 °F | |
Mallard Creek Polymers Rovene® 6506 Styrene-Acrylic Emulsion Applications: Rovene® 6506 typical applications are across a variety of nonwoven markets and substrates. Rovene® 6506 has demonstrated excellent performance as a binder on a lightweight nonwov.. |
|||
Glass Transition Temp, Tg | -10.0 °C | 14.0 °F | |
Styron XZ 92089.01 Cross-Linking SB Performance Features: Excellent alkali resistance, low blockingApplications: Fiber Binding, Glass Fiber Binding and Performance CoatingsEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -10.0 °C | 14.0 °F | |
Styron XZ 95047.00 Carboxylated SB Performance Features: FDA compliant sealant, excellent water resistanceApplications: General Purpose AdhesiveEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -10.0 °C | 14.0 °F | DSC |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Glass Transition Temp, Tg | -10.0 °C | 14.0 °F | |
Unitika elitel UE3700 Polyester, Pellet Hot melt adhesives, Adhesives for fibers, Adhesives for interlining clothsUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from p.. |