Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 530A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate
(discontinued **) Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
(discontinued **) Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |