Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | Average value: 1.34 J/g-°C Grade Count:3 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Specific Heat Capacity | 1.34 - 1.76 J/g-°C | 0.320 - 0.421 BTU/lb-°F | Average value: 1.54 J/g-°C Grade Count:3 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | ASTM D3418 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |
|||
Specific Heat Capacity | 1.34 J/g-°C @Temperature 25.0 °C |
0.320 BTU/lb-°F @Temperature 77.0 °F |
Liquid |
Asahi Glass ASAHIKLIN AK-225T Hydrochlorofluorocarbon Solvent AK-225T is a mixture of AK-225, ethanol, hydrocarbon and stabilizers. This blend was developed for those customers needing a more aggressive defluxer than AK_225AES. It has proven to be effective in.. |