Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.23 J/g-°C | 0.294 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |