Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.690 J/g-°C @Temperature 0.000 - 50.0 °C |
0.165 BTU/lb-°F @Temperature 32.0 - 122 °F |
|
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.689 J/g-°C @Temperature 900 °C |
0.165 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-BAK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-BALF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-FK51A Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-SF6 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-SF6HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | ASTM-E1269 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |