Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.137 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy plate, 1000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 10% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 20% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 40% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Specific Heat Capacity 0.573 J/g-°C

@Temperature 900 °C
0.137 BTU/lb-°F

@Temperature 1650 °F
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.575 J/g-°C

@Temperature 1000 °C
0.137 BTU/lb-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.575 J/g-°C

@Temperature 1000 °C
0.137 BTU/lb-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.575 J/g-°C

@Temperature 1000 °C
0.137 BTU/lb-°F

@Temperature 1830 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.574 J/g-°C
0.137 BTU/lb-°F
Schott N-SSK5 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, plate, 16000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy plate, 8000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 50% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Specific Heat Capacity 0.574 J/g-°C

@Temperature 700 °C
0.137 BTU/lb-°F

@Temperature 1290 °F
Haynes 230® alloy, as cast vacuum investment casting
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Copyright © lookpolymers.com All Rights Reserved