Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | RT |
Outokumpu 4713 High Temperature Ferritic Stainless Steel Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 300 °C |
0.103 BTU/lb-°F @Temperature 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 400 °C |
0.103 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 400 °C |
0.103 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.431 J/g-°C | 0.103 BTU/lb-°F | |
Special Metals INCOLOY® Alloy 907 A nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of INCOLOY alloy 903 but with improved notch.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Special Metals Nickel 212 Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow.. |
|||
Specific Heat Capacity | 0.431 J/g-°C | 0.103 BTU/lb-°F | |
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |
|||
Specific Heat Capacity | 0.430 - 0.470 J/g-°C | 0.103 - 0.112 BTU/lb-°F | as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Specific Heat Capacity | 0.430 - 0.470 J/g-°C | 0.103 - 0.112 BTU/lb-°F | after age hardening |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range) 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.Ge.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Specific Heat Capacity | 0.430 J/g-°C | 0.103 BTU/lb-°F | |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Annealed Plate, Sheet, and Strip, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Specific Heat Capacity | 0.431 J/g-°C @Temperature 400 °C |
0.103 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |