Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Dow Corning XIAMETER® PMCPPMX-200 5CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 5CS. 100% active, 5 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-26B Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-30B Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-28H Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-32 Samarium Cobalt Magnetic Material |
|||
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Alliance S-26H Samarium Cobalt Magnetic Material |