Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.130 J/g-°C | 0.0311 BTU/lb-°F | Solid |
Indium Corp. Indalloy 200 Pure Gold Information Provided by Indium Corporation |
|||
Specific Heat Capacity | 0.130 J/g-°C | 0.0311 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation. |