Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 - 2.10 J/g-°C | 0.359 - 0.502 BTU/lb-°F | Average value: 1.70 J/g-°C Grade Count:5 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Specific Heat Capacity | 2.00 - 2.10 J/g-°C | 0.478 - 0.502 BTU/lb-°F | Average value: 2.01 J/g-°C Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |