Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.28 J/g-°C | 0.306 BTU/lb-°F | |
LG Chemical Phenol Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati.. |
|||
Specific Heat Capacity | 1.28 - 1.73 J/g-°C @Temperature 50.0 - 200 °C |
0.306 - 0.413 BTU/lb-°F @Temperature 122 - 392 °F |
Average value: 1.50 J/g-°C Grade Count:2 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |