Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.17 J/g-°C @Temperature 70.0 °C |
0.280 BTU/lb-°F @Temperature 158 °F |
ASTM D648 |
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Specific Heat Capacity | 1.17 - 1.81 J/g-°C @Temperature 50.0 - 200 °C |
0.280 - 0.433 BTU/lb-°F @Temperature 122 - 392 °F |
Average value: 1.51 J/g-°C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Specific Heat Capacity | 1.17 J/g-°C @Temperature 1100 °C |
0.280 BTU/lb-°F @Temperature 2010 °F |
|
Zircar Ceramics ASB-2600 Alumina-Silica Blanket Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | ASTM D2766 |
Covestro Makrolon® 2607 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially a.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | ASTM D2766 |
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® ADS Polyester Film, 500 Gauge Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® EB11 Polyester Film, 200 Gauge Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® EL Polyester Film, 75 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® HP Polyester Film, 36 Gauge Mylar® HP film is a high strength, high clarity and low haze polyester film with dimensional stability particularly suitable for use in applications where dimensional stability is a requirement dur.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® HP Polyester Film, 48 Gauge Mylar® HP film is a high strength, high clarity and low haze polyester film with dimensional stability particularly suitable for use in applications where dimensional stability is a requirement dur.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® OWF Polyester Film, 120 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® OWF Polyester Film, 48 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® RSX Polyester Film, 175 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® RSX Polyester Film, 500 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® RSX Polyester Film, 92 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 120 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® WC Polyester Film, 48 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® M461 Polyester Film, 300 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® MDA Polyester Film, 400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® WC Polyester Film, 300 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® LJP Polyester Film, 300 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® WC Polyester Film, 400 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 142 Gauge Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin.. |
|||
Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |