Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Momentive Performance Materials HBT Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Schott N-FK5 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |