Polymer Property : Specific Heat Capacity = 0.790 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Calculated
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
Specific Heat Capacity 0.790 - 0.830 J/g-°C
0.189 - 0.198 BTU/lb-°F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.790 - 1.00 J/g-°C
0.189 - 0.239 BTU/lb-°F
Average value: 0.910 J/g-°C Grade Count:12
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Schott LITHOSIL-Q Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Schott N-SF2 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Schott P-SF8 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Corning Macor® Machinable Glass Ceramic
The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,..
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Accuratus MACOR Machinable Glass Ceramic
Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac..
Specific Heat Capacity 0.790 J/g-°C

@Temperature 50.0 °C
0.189 BTU/lb-°F

@Temperature 122 °F
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic
“Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli..
Specific Heat Capacity 0.790 J/g-°C
0.189 BTU/lb-°F
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and ..