Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.480 J/g-°C @Temperature 20.0 °C |
0.115 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
Specific Heat Capacity | 0.480 J/g-°C @Temperature 20.0 °C |
0.115 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Specific Heat Capacity | 0.480 J/g-°C | 0.115 BTU/lb-°F | |
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |