Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due .. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Weartech International WT-50 Nickel Hardfacing & Wear Resistant Alloy Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applicationsInformation provided by Weartech International |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.Applications: Taps, twist drills, reamers, broaching tools, meta.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, 1149°C (2100°F) Solution Treated, UNS N06601 Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600 Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276) TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numero.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |