Thermal Properties Metric English Comments
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 1000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Specific Heat Capacity 0.403 J/g-°C
0.0963 BTU/lb-°F
RT
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..