Polymer Property : Specific Heat Capacity = 0.201 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.201 J/g-°C

@Temperature 20.0 °C
0.0480 BTU/lb-°F

@Temperature 68.0 °F
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite
RWMA Class 11.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a hard..
Specific Heat Capacity 0.201 J/g-°C
0.0480 BTU/lb-°F
Liquid
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m..
Specific Heat Capacity 0.201 J/g-°C
0.0480 BTU/lb-°F
Liquid
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy
General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation.